How do you tan a racoon hide?

Use finishing nails to attach the corners of the hide to the wood. Scrape the visible flesh from the hide with a sharp knife. Cut a slit down the tail and scrape any flesh from the inside of the tail. Pour one pound of noniodized salt on the hide and use your hands to lightly rub it into every part of the exposed skin.

How much does it cost to tan a raccoon hide?

Standard Tanning 75+ PELTS 11 to 74 FUR TYPE $13.00 $17.50 Raccoon, Skunk $16.50 $19.00 Red Fox, Grey Fox, Fisher $20.00 $24.00 Badger, Coyote, Farm Fox $22.50 $25.00 *Bobcat, *Lynx, *Otter (*Must have CITES tag on pelts).

Can you tan a hide with just salt?

Use 1/2 lb of table salt per gallon of water and extremely hot water to dissolve the salt. Mix thoroughly until salt is dissolved and let the water cool. Immerse the hide in the solution and leave for six to eight hours. Overnight is fine, but if you leave it too long, the hair will start falling off the hide.

How do you tan a raccoon hide with alum?

In a separate container, dissolve 4 ounces of Sodium Carbonate and 1 cup of salt to every ½ gallon of water. Very slowly pour the soda and salt solution in the alum solution and stir very well. Immerse the skins and stir frequently. Light skinned animals such as Squirrel, Bobcat, Fox, or Coyote will tan in 48 hours.

How do you tan a raccoon hide with borax?

Coat the inside of the pelt with the Borax paste, using a knife to spread it to a thickness of 1/8 inch. Put on rubber gloves and work the paste with your fingers, rubbing it firmly into the skin. Leave the paste on the skin until the next day, then scrape it off and apply another coating.

How do you tan a beaver hide?

Create a tanning solution by boiling oak or another similar bark in water until the water is dark brown or black. This releases tannins into the water, which will cure your hide. Rub the tanning solution into the hairless side of your pelt until it is dry. Repeat.

Can you sell raccoon fur?

You could expect to get $30 for it when you go to sell it, maybe less for small raccoons depending on the buyer. You might get $5 for a finished ‘coon at auction, if it is in the absolute best condition.

How much is a beaver pelt worth?

With beavers, the work starts as soon as you get out of the truck. Pelt prices for beaver should be about what they have been in the last few years: $10 to $15 for a good prime blanket. Raccoon – Like beaver, they take more effort to prepare than other pelts. Expect the usual $10 to $15 for a good, big, heavy pelt.

How much is a coyote pelt worth?

Southern and lower quality coyote pelts may get $10-15. Muskrat pelts have seen decent demand lately and are one of the only fur items that have actually increased in price over the past years.

Can you tan a hide with olive oil?

Coconut oil, olive oil, almond oil, or vegetable oil can also be used. Some tanners apply oil both before and after smoking to help ensure the leather does not dry out too much and crack during the smoking process.

How long will a salted hide last?

Will store at least one year. This is the most practical method for people who tan alot of hides. Storing salted hides in tarps or other permeable containers causes them to dry slowly over time. The more they dry the harder they will be to scrape later.

What does Borax do to a hide?

Borax is used for soaking hides and skins, for stripping vegetable tans and for neutralizing chrome tans. Boric acid is used mainly for neutralizing limed pelts. Hides and skins are usually cured by drying or salting to preserve them during storage or transportation before they are tanned.

How do you make homemade tanning lotion?

Instructions: Start out by combining 1/2 cup of unscented white lotion in a bowl with 1/3 cup of pure cocoa powder. Mix with a fork. Make sure to break up any clumps and blend well. Adjust the recipe to match your desired color. Smooth the tanning lotion over your entire body evenly. Apply daily for a gradual deep tan.

How do you make a hide tan formula?

Dissolve 2 ½ pounds of salt in 4 gallons of water in the garbage can. In a plastic bucket, dissolve 1 pound of ammonia alum in a gallon of water. Slowly pour the alum solution into the garbage can, mixing thoroughly. Soak the deer hide for four days, occasionally stirring to make sure it’s well coated.

How does alum tanning work?

After tanning with alum, the dried leather is stiff and firm. To make it softer, the leather is then tumbled and greased. Alum tanning makes the leather white and very water-sensitive.

How do you tan hides without chemicals?

Overview of how to tan a hide by brain tanning Evaluate the hide and trim off edges. Remove the flesh. Soak in water or a bucking solution. Scrape off grain and membrane. Wring out moisture. Apply braining solution. Wring hide. Repeat braining and wringing.

Do you have to dry a hide before tanning?

Use clean water and soap made from natural substances to wash away dirt, blood, and other impurities before you begin softening the skin. Dry the hide. Let it dry out for a few days to prepare it for the tanning process. Make sure that the hide is actually stretched, not just hung, on the drying rack.