The side that sticks to the moisture on your finger or thumb is the side which is water soluble and this is the side which faces down in the water.

Do You Use warm or cold water for hydro dipping?

The ideal water temperature range for hydrographic dipping is 80 to 90 degrees Fahrenheit. Some dip manufacturers may recommend a specific temperature, such as 80 degrees.

Do you have to clear coat after hydro dipping?

STEP 11: CLEAR COAT Clear coating is highly recommended for all hydrographically decorated parts. This helps to seal in the inks and allows for a cleaner finished product. When the dipped part is dry, apply the clear top coating (matte, semi-gloss or high gloss) to finish off your newly dipped hydrographic part.

What is Hydrographic activator?

Activator is the key element in the hydro dipping process. It is a chemical so integral to the process of hydro dipping that it acts as a key difference between successful and unsuccessful dips. The activator is applied to the film to make it dissolve and turn the film ink into liquid.

What clear coat do you use for hydro dipping?

TWN’s clear coats are specifically designed for hydrographics. No matter your project or application, we have a clear coat with the unique characteristics that you need to create a long-lasting finish. CCI clear coats are the ultimate clear coat for sporting goods items.

Do you need activator to Hydro dip?

Under and over activating are two of the leading causes in problems with hydro dipping. You are not applying a layer of paint, you just need enough activator (with a fine mist, fan pattern spray) to cover the film lightly. We recommend HydroVator with all out films.

How do you activate hydro dip film?

To do the test wet your index and thumb finger and pinch the film on the corner, the side that sticks to your fingers is the PVA side and this side goes down on the water. Spray your Hydrovator Activator evenly at a steady pace. We recommend doing one even coat. Watch for the film expand and glass over.

Do you have to prime before hydro dipping?

Dupli-Color Primer The first necessary ingredient to hydro dipping is the primer. It promotes adhesion of the transfer film to the object. After applying the primer, allow for it to dry, before transfering a film onto your part. This can take up to two hours.

Can you hydro dip twice?

Sometimes you’re not happy with your initial hydro dip so you want to give it another coat to cover up the old paint. Or maybe you want to dip more than once to merge multiple graphics and create cool effects. If you’re going to do this make sure your product is dry before dipping again.

How long does it take hydro dipping to dry?

Step 2: Paint the Base Coat Be sure to avoid any fingerprints for a smooth finish, and avoid spraying the concrete at school to keep everyone happy in the process. After a full base coat is applied, it will take about 24 hours for the paint to dry.

How long after hydro dipping can I clear coat?

The clear coat should be allowed to dry for at least 8-24 hours. Your item will be ready to use when the clear coat is no longer tacky to the touch and has sufficient time to fully cure out.

What is activator for hydro dipping?

What the Activator Is. The activator is a chemical that liquefies the ink on the hydro dip film. After you have primed the object and painted it, the item is ready for the film. This liquefies the ink on the surface of the water.

What causes bubbles in hydro dipping?

When the film was placed on the water, air bubbles have come under the film. In places where bubbles are the film does not adhere. You can try to gently push away the air bubbles under the film (immediately after the deposit and with a latex glove). Because the dipping angle was not right, small bubbles remain.

What is activator A?

Some chiropractors use a small, hand-held instrument called the Activator Adjusting Instrument to deliver a quick, low-force impulse to spinal joints with the goal of restoring motion to the targeted joint.

How does water transfer printing work?

The process utilizes a water-soluble film that contains the printed patterns. The film dissolves in the water and leaves the ink on the surface. In the typical process, the item to be printed is first coated with a primer or an adhesion promoter. The item then is dipped into the water, and the ink wraps around it.

How tough is hydro dipping?

Hydrographic finishes are very robust and will last for many years under normal use. However, similar to your car finish, the paint can scratch if the product is abused. Scratching the protective clear coat can cause failure to the hydrographic finish.

Can you hydro dip a car?

His latest clip was brought to our attention by TheDrive, and it shows the hydro dipping of a complete car. With no disassembling. Yes, it’s possible.

Can I Hydrodip at home?

Fill the plastic container with warm water to a level that is high enough to submerge your object without water spilling over the sides. Put on the gloves, and slowly dip the object into the water at an angle until it is completely submerged; do not let go of the object.

How expensive is hydro dipping?

Average Costs for Hydro Dipping The average cost for hydro dipping a wheel for a vehicle is roughly $150, and that pricing can vary by as much as 20% – 50%, depending on the type of activator, finish, and labor costs. Hydro dipping fees for guns typically range from $200 to $500, depending on the make and model.

Can u hydro dip glass?

These hydro dip glass bottles are colorful and unique and the paint technique is easy. You will never get the same paint finish twice with hydro dipping. I have photos, a tutorial, and a video showing the process. Definitely watch the video because the technique is so much easier to follow.